Sign In | Join Free | My himfr.com
Home > Boron Doped Diamond >

CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color

Shaper Diamond Technology Co., Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now
    Buy cheap CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color from wholesalers
     
    Buy cheap CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color from wholesalers
    • Buy cheap CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color from wholesalers
    • Buy cheap CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color from wholesalers
    • Buy cheap CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color from wholesalers
    • Buy cheap CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color from wholesalers

    CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color

    Ask Lasest Price
    Brand Name : Infi
    Model Number : Null
    Certification : Non Certificate
    Price : To be negotiated
    Payment Terms : T/T, Western Union, PayPal
    Supply Ability : 100pcs/7days
    Delivery Time : 7 working days
    • Product Details
    • Company Profile

    CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color

    CVD Polycrystalline Boron-Doped Diamond BDD CVD Diamond

    The BDD electrode uses boron-doped diamond film as the electrode anode, and titanium or other materials as the cathode for electrolysis. The special sp3 bond structure of boron-doped diamond film and its electrical conductivity give the diamond film electrode excellent electrochemical characteristics, extremely high oxygen evolution potential and widest electrochemical window, lower background current, and better physical and chemical stability and low adsorption characteristics. It is an ideal anode material for electrochemical oxidation treatment of hard-to-biodegrade organic wastewater.


    Product details:

    Crystal growth process:cvd Boron-doped
    Color:black
    Shape:Circle ,Square,triangle
    Application

    various organic waste water, such as organic waste water in the fields of medicine /agrochemicals,petrochemicals, coking, smelting, printing and dyeing,papermaking, tanning, explosives, wine making, landfill leachate, etc.

    Application noteProperties of BDD are particularly important in electroanalysis for the development of sensors and biosensors. BDD electrodes allow to detect many electroactive molecules in aqueous media that would otherwise be masked by water decomposition reactions at higher potentials. The surface of BDD electrode can be further (photo)functionalized or decorated. In order to enhance the electrochemical response in a presence of organic molecules, the surface of BDD can be also modified with metal nanoparticles (e.g. Au). BDD is also a broadly used electrode material for electrochemical energy storage, electrocatalysis or electrosynthesis.
    Please note that two larger surfaces have non-equal properties. This is a consequence of postprocessing of BDD polycrystal. While one surface is just polished the second is first laser cut and then polished. The temperature released during the laser cut affects the level of boron doping and in consequence decrease the conductivity. Chemical etching is recommended before use.
    Orientation:4pt/100
    Key product features:BDD is a semi-metallic material characterized by high conductivity and fast electron transfer. BDD electrodes are recognized as being superior to other electrode materials due to excellent electrochemical properties.
    Main advantages include:
    (1) outstanding chemical and dimensional stability,
    (2) exceptionally low background current,
    (3) an extremely wide potential window for water electrolysis,
    (4) a broad electromagnetic transparency window of thin films ranging from the UV-Vis region to the far-infrared region,
    (5) low magnetic susceptibility compared to other electrode materials,
    and (vi) excellent biocompatibility (sp3 hybridized structure).
    Under the same conditions, the efficiency and energy consumption of BDD electrodes in degrading organics are significantly better than other electrodes.
    thickness tolerance:< 10%
    expected potential window in aqueous media:~3.0 - 3.5 V
    expected potential window in organic media:~5.0 - 7.5 V
    expected capacitance (after chemical etching):~10 µF cm2
    measured B doping level:1.4·1020 cm3 (side A), 4.5·1020 cm3 (side B)
    measured resistivity:9 ohm·cm (side B), 15 ohm·cm (side A)

    Packing and shipping:

    Selling Units:Single item
    Single package size:20X15X15cm
    Port:Changsha
    Single gross weight:0.100 kg

    Package: small sealed plastic bag and carton(strong and safe package) Delivery: usually 3-7 working days after the payment confirmation


    Transportation: DHL, TNT, Fedex, UPS or as per your request.


    Quality CVD Polycrystalline Bdd Diamond Boron Doped 4pt / 100 Orientation Black Color for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Shaper Diamond Technology Co., Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)